Superalloys – Engineered to Perform at Extreme Temperatures
High-performance nickel, cobalt and iron-based superalloys designed for high-temperature, high-stress, and corrosive industrial environments. Trusted by aerospace, energy and chemical industries.
What Are Superalloys?
Superalloys, also known as high-performance alloys, are a class of metallic materials designed to:
Maintain strength and surface stability at temperatures above 600°C (1110°F)
Resist oxidation, creep, fatigue and corrosion under stress
Serve in aerospace, turbine engines, nuclear, and chemical plants
Superalloy Categories:
Type | Base Metal | Typical Grades | Applications |
---|---|---|---|
Nickel-based | Ni | Inconel 625, 718, X750 | Turbines, heat exchangers |
Cobalt-based | Co | Haynes 25, L605, 188 | Jet engines, combustors |
Iron-based | Fe | A-286, Incoloy 800/825 | Petrochemicals, heat tubes |
These alloys combine solid solution strengthening, precipitation hardening, and oxidation resistance to achieve unmatched reliability in harsh environments.
Products Link

- Alloy >>
- Heat-Resistant Steel
- Inconel Alloys
- Urea-Grade Steel
- Titanium Alloys
- Superalloys
- Super Duplex Stainless Steels
- Special Stainless Steels
- Soft Magnetic Alloys
- Precipitation Hardening Stainless
- Hydropower Steel
- Incoloy Alloys
- Super Austenitic Stainless Steels
- High-Strength Steels
- Monel Alloys
- Hastelloy Alloy
- Cobalt Based Alloy
- Stainless Steel >>
- Galvanized Steel >>
- Carbon Steel >>
- Aluminum Steel >>
Optional product specifications
Property | Details |
---|---|
Grades Available | Inconel 625, 718, X750, C-276, Haynes 188, Monel 400, A286, Incoloy 800/825, Waspaloy |
Standards | ASTM B564, B637, B168, AMS, NACE MR0175 |
Forms | Sheet, plate, round bar, rod, wire, tube, pipe, forging |
Heat Treatment | Solution Annealed, Aged (e.g. 718 – AMS 5662/5663) |
Sizes | |
• Plate: 1.5mm – 80mm | |
• Bar: Ø6mm – Ø250mm | |
• Pipe: 1/2" – 12", SCH 10–XXS | |
Delivery Condition | As-forged, solution-treated, or aged |
* Third-party testing: PMI, UT, X-ray, grain size, hardness, tensile, stress rupture
Processing & Packaging

Cut to length, block cutting, centerless grinding

Solution annealing & aging services per AMS

Eddy current, ultrasonic, radiographic testing

Heat number + spec + QR code markings

Wooden crates + vacuum / foil wrap + VCI paper
Why Buy From Xishang?
- Complete range of Ni, Co, Fe-based superalloys
- Support for AMS / ASTM / NACE / ISO standards
- CNC Machining, heat treatment, forging & cut-to-size
- Full traceability with MTC, grain size & microstructure reports
- Export-grade packaging and fast global logistics
- Custom trial production for critical OEMs or EPC projects
Frequently Asked Questions
Q1: Which superalloy is best for 700°C continuous service?
A:
Inconel 625 or 617 are ideal due to high strength and oxidation resistance at 650–800°C range.
Q2: Can I get heat treatment per AMS specifications?
A:
Yes, we support AMS 5662, 5663 (for Inconel 718) and other heat treatment cycles on request.
Q3: Do you offer non-standard bar sizes?
A:
We offer forged or rolled bars in custom diameters and lengths with tight tolerances.
Q4: Can you machine complex turbine shapes?
A:
Yes, CNC and EDM services are available for superalloy components per drawing.
Q5: What is the lead time for superalloy plate or forged parts?
A:
Stock items: 5–7 days. Forged or heat-treated: 10–25 days based on grade and complexity.